新型Ni-Co基高温合金塑性变形连接中界面组织演化及愈合机制 |
| 任少飞, 张健杨, 张新房, 孙明月, 徐斌, 崔传勇 |
|
Evolution of Interfacial Microstructure of Ni-Co Base Superalloy During Plastic Deformation Bonding and Its Bonding Mechanism |
| REN Shaofei, ZHANG Jianyang, ZHANG Xinfang, SUN Mingyue, XU Bin, CUI Chuanyong |
| 图10 塑性变形连接界面愈合机制 (a) original coarse grains (b, c) grain refinement near the interface (d, e) bulging of the interfacial grains (Fig.10e shows the recrystallization nucleation of interfacial grains) (f) bonding of the interface |
| Fig. 10 Interface bonding mechanism during plastic deformation bonding |
|