新型Ni-Co基高温合金塑性变形连接中界面组织演化及愈合机制 |
| 任少飞, 张健杨, 张新房, 孙明月, 徐斌, 崔传勇 |
|
Evolution of Interfacial Microstructure of Ni-Co Base Superalloy During Plastic Deformation Bonding and Its Bonding Mechanism |
| REN Shaofei, ZHANG Jianyang, ZHANG Xinfang, SUN Mingyue, XU Bin, CUI Chuanyong |
| 图3 应变速率为0.001 s-1,不同变形温度下Ni-Co基高温合金显微组织的OM像及其流变应力-应变曲线 |
| Fig.3 OM images of microstructures at deformation temperatures of 1000oC (a), 1050oC (b), 1100oC (c), 1150oC (d), and 1200oC (e), and the true stress-strain curves (f) of the Ni-Co base superalloy at the strain rate of 0.001 s-1 |
|