新型Ni-Co基高温合金塑性变形连接中界面组织演化及愈合机制 |
| 任少飞, 张健杨, 张新房, 孙明月, 徐斌, 崔传勇 |
|
Evolution of Interfacial Microstructure of Ni-Co Base Superalloy During Plastic Deformation Bonding and Its Bonding Mechanism |
| REN Shaofei, ZHANG Jianyang, ZHANG Xinfang, SUN Mingyue, XU Bin, CUI Chuanyong |
| 图5 不同变形量下接头的室温拉伸曲线 |
| Fig.5 Tensile curves of the joints at room temperature under different deformations |
|