GH4169合金拘束相关的疲劳裂纹萌生寿命 |
| 郭昊函, 杨杰, 刘芳, 卢荣生 |
|
Constraint Related Fatigue Crack Initiation Life of GH4169 Superalloy |
| GUO Haohan, YANG Jie, LIU Fang, LU Rongsheng |
| 图14 累积塑性滑移与循环周次间的关系 |
| Fig.14 Relationships between accumulated plastic slip and cycle number (a) |
|