GH4169合金拘束相关的疲劳裂纹萌生寿命 |
| 郭昊函, 杨杰, 刘芳, 卢荣生 |
|
Constraint Related Fatigue Crack Initiation Life of GH4169 Superalloy |
| GUO Haohan, YANG Jie, LIU Fang, LU Rongsheng |
| 图2 模型加载与尺寸示意图 |
| Fig.2 Schematic of model loading and geometry (a—micro-notch depth, b—micro-notch length, RP—reference point) |
|