Q235和Q450NQR1在中国南沙海洋大气环境中暴晒34个月后的腐蚀行为 |
| 刘雨薇, 顾天真, 王振尧, 汪川, 曹公望 |
|
Corrosion Behavior of Q235 and Q450NQR1 Exposed to Marine Atmospheric Environment in Nansha, China for 34 Months |
| LIU Yuwei, GU Tianzhen, WANG Zhenyao, WANG Chuan, CAO Gongwang |
| 图8 Q235和Q450NQR1的应力-应变曲线 |
| Fig.8 Stress (σ)-strain (ε) curves of Q235 (a) and Q450NQR1 (b) exposed for different periods |
|