Q235和Q450NQR1在中国南沙海洋大气环境中暴晒34个月后的腐蚀行为 |
| 刘雨薇, 顾天真, 王振尧, 汪川, 曹公望 |
|
Corrosion Behavior of Q235 and Q450NQR1 Exposed to Marine Atmospheric Environment in Nansha, China for 34 Months |
| LIU Yuwei, GU Tianzhen, WANG Zhenyao, WANG Chuan, CAO Gongwang |
| 图4 Q235和Q450NQR1表面锈层的宏观形貌 |
| Fig.4 Macro-morphologies of the rust layer on skyward (a-d) and field-ward (e-h) sides of Q235 and Q450NQR1 (Arrows show local peeling of rust layer) (a, e) Q235, 21 months (b, f) Q235, 34 months (c, g) Q450NQR1, 21 months (d, h) Q450NQR1, 34 months |
|