Fe13Cr5Al4Mo合金在高温高压水环境中的腐蚀行为 |
||||||||||||||||||
| 林晓冬, 马海滨, 任啟森, 孙蓉蓉, 张文怀, 胡丽娟, 梁雪, 李毅丰, 姚美意 | ||||||||||||||||||
|
Corrosion Behaviors of Fe13Cr5Al4Mo Alloy in High-Temperature High-Pressure Water Environments |
||||||||||||||||||
| LIN Xiaodong, MA Haibin, REN Qisen, SUN Rongrong, ZHANG Wenhuai, HU Lijuan, LIANG Xue, LI Yifeng, YAO Meiyi | ||||||||||||||||||
| 表1 Fe13Cr5Al4Mo合金的名义和实测成分 (mass fraction / %) |
||||||||||||||||||
| Table 1 Nominal and measured chemical compositions of Fe13Cr5Al4Mo alloy |
||||||||||||||||||
|
||||||||||||||||||