Fe13Cr5Al4Mo合金在高温高压水环境中的腐蚀行为 |
| 林晓冬, 马海滨, 任啟森, 孙蓉蓉, 张文怀, 胡丽娟, 梁雪, 李毅丰, 姚美意 |
|
Corrosion Behaviors of Fe13Cr5Al4Mo Alloy in High-Temperature High-Pressure Water Environments |
| LIN Xiaodong, MA Haibin, REN Qisen, SUN Rongrong, ZHANG Wenhuai, HU Lijuan, LIANG Xue, LI Yifeng, YAO Meiyi |
| 图3 Fe13Cr5Al4Mo和Zr-4合金在去离子水和Li + B水溶液中的腐蚀增重曲线 |
| Fig.3 Weight gain curves of Fe13Cr5Al4Mo and Zr-4 alloys exposed to deionized water and Li + B aqueous solution |
|