基板表层组织对Fe-16Mn-0.7C-1.5Al TWIP钢可镀性的影响 |
| 彭俊, 金鑫焱, 钟勇, 王利 |
|
Influence of Substrate Surface Structure on the Galvanizability of Fe-16Mn-0.7C-1.5Al TWIP Steel Sheet |
| PENG Jun, JIN Xinyan, ZHONG Yong, WANG Li |
| 图15 基板表层组织对TWIP钢可镀性的影响示意图 |
| Fig.15 Schematics of the influence of substrate surface structure on galvanizability of TWIP steel (TWIP—twinning induced plasticity steel)(a) as received cold rolled steel(b) pretreated steel having a ferrite surface layer |
|