基板表层组织对Fe-16Mn-0.7C-1.5Al TWIP钢可镀性的影响 |
| 彭俊, 金鑫焱, 钟勇, 王利 |
|
Influence of Substrate Surface Structure on the Galvanizability of Fe-16Mn-0.7C-1.5Al TWIP Steel Sheet |
| PENG Jun, JIN Xinyan, ZHONG Yong, WANG Li |
| 图11 镀锌试样截面形貌 |
| Fig.11 Cross-sectional morphologies of the hot dip galvanized samples (a) sample A (b) sample B |
|