基板表层组织对Fe-16Mn-0.7C-1.5Al TWIP钢可镀性的影响 |
| 彭俊, 金鑫焱, 钟勇, 王利 |
|
Influence of Substrate Surface Structure on the Galvanizability of Fe-16Mn-0.7C-1.5Al TWIP Steel Sheet |
| PENG Jun, JIN Xinyan, ZHONG Yong, WANG Li |
| 图10 镀锌试样溶掉锌层后基板表面形貌SEM像 |
| Fig.10 SEM images of the substrate surfaces of samples A (a, b) and B (c-e) after the zinc coating was stripped |
|