基板表层组织对Fe-16Mn-0.7C-1.5Al TWIP钢可镀性的影响 |
| 彭俊, 金鑫焱, 钟勇, 王利 |
|
Influence of Substrate Surface Structure on the Galvanizability of Fe-16Mn-0.7C-1.5Al TWIP Steel Sheet |
| PENG Jun, JIN Xinyan, ZHONG Yong, WANG Li |
| 图9 退火试样表面SEM形貌及EDS分析结果 |
| Fig.9 Surface SEM morphologies (a, b) and their EDS spectra (c, d) of the annealed samples A (a, c) and B (b, d) |
|