钒微合金化中锰马氏体耐磨钢奥氏体晶粒长大行为 |
| 韩汝洋, 杨庚蔚, 孙新军, 赵刚, 梁小凯, 朱晓翔 |
|
Austenite Grain Growth Behavior of Vanadium Microalloying Medium Manganese Martensitic Wear-Resistant Steel |
| HAN Ruyang, YANG Gengwei, SUN Xinjun, ZHAO Gang, LIANG Xiaokai, ZHU Xiaoxiang |
| 图9 试样中V(C, N)粒子的平均直径随温度的变化 |
| Fig.9 Variations of the average size of V(C, N) with heating temperatures in the samples |
|