表1 不同温度下保温600、1800和3600 s后试样中第二相粒子体积分数 (volume fraction / %)
Table 1 Volume fractions of second phase particles of samples after holding at different heating temperatures for 600 s, 1800 s, and 3600 s
Time / s820oC850oC900oC950oC
6000.315 ± 0.0250.231 ± 0.0320.126 ± 0.0360.049 ± 0.013
18000.273 ± 0.0370.211 ± 0.0330.086 ± 0.0290.037 ± 0.012
36000.265 ± 0.0430.169 ± 0.0380.046 ± 0.0210.023 ± 0.006