热输入对Q500qE钢模拟CGHAZ微观组织和冲击韧性的影响
朱东明, 何江里, 史根豪, 王青峰

Effect of Welding Heat Input on Microstructure and Impact Toughness of the Simulated CGHAZ in Q500qE Steel
ZHU Dongming, HE Jiangli, SHI Genhao, WANG Qingfeng
图9 不同热输入下CGHAZ的热膨胀曲线以及对应的奥氏体向铁素体转变开始温度
Fig.9 Expansion curves and Ar3 of CGHAZs with different heat inputs (Ar3—the starting temperature for γ→α transformation)