热输入对Q500qE钢模拟CGHAZ微观组织和冲击韧性的影响 |
| 朱东明, 何江里, 史根豪, 王青峰 |
|
Effect of Welding Heat Input on Microstructure and Impact Toughness of the Simulated CGHAZ in Q500qE Steel |
| ZHU Dongming, HE Jiangli, SHI Genhao, WANG Qingfeng |
| 图1 Q500qE钢板的原始组织 |
| Fig.1 Original microstructure of the Q500qE steel plate |
|