磁场与晶粒尺寸协同作用对马氏体形核及变体选择的影响 |
| 原家华, 张秋红, 王金亮, 王灵禺, 王晨充, 徐伟 |
|
Synergistic Effect of Magnetic Field and Grain Size on Martensite Nucleation and Variant Selection |
| YUAN Jiahua, ZHANG Qiuhong, WANG Jinliang, WANG Lingyu, WANG Chenchong, XU Wei |
| 图3 不同晶粒尺寸SUS321不锈钢施加1和9 T磁场作用经连续冷却处理后显微组织的EBSD相图 |
| Fig.3 EBSD phase maps of microstructure evolution of SUS321 stainless steel with different grain sizes during cooling under 1 T (a, c, e) and 9 T (b, d, f) magnetic fields (a, b) 6.6 μm (c, d) 29.3 μm (e, f) 203 μm |
|