回火温度对1000 MPa级NiCrMoV低碳合金钢微观组织和低温韧性的影响 |
| 周成, 赵坦, 叶其斌, 田勇, 王昭东, 高秀华 |
|
Effects of Tempering Temperature on Microstructure and Low-Temperature Toughness of 1000 MPa Grade NiCrMoV Low Carbon Alloyed Steel |
| ZHOU Cheng, ZHAO Tan, YE Qibin, TIAN Yong, WANG Zhaodong, GAO Xiuhua |
| 图 11 NiCrMoV低碳合金钢在500℃回火时析出相的TEM像及其对应的EDS |
| Fig.11 TEM image (a) and corresponding EDS result (b) of precipitates of the NiCrMoV low carbon alloyed steel tempered at 500oC |
|