回火温度对1000 MPa级NiCrMoV低碳合金钢微观组织和低温韧性的影响 |
| 周成, 赵坦, 叶其斌, 田勇, 王昭东, 高秀华 |
|
Effects of Tempering Temperature on Microstructure and Low-Temperature Toughness of 1000 MPa Grade NiCrMoV Low Carbon Alloyed Steel |
| ZHOU Cheng, ZHAO Tan, YE Qibin, TIAN Yong, WANG Zhaodong, GAO Xiuhua |
| 图10 利用DICTRA模拟NiCrMoV低碳合金钢在两相区回火过程中合金元素配分过程 |
| Fig.10 Alloying element partitioning process of the NiCrMoV low carbon alloyed steel in two-phase region tempering by DICTRA simulation (a) dimensional model of partitioning process (b) evolution of reversed austenite volume fraction (NPLE—negligible partition local equilibrium, PLE—partition local equilibrium) (c) C distribution (d) Ni distribution (e) Mn distribution |
|