回火温度对1000 MPa级NiCrMoV低碳合金钢微观组织和低温韧性的影响 |
| 周成, 赵坦, 叶其斌, 田勇, 王昭东, 高秀华 |
|
Effects of Tempering Temperature on Microstructure and Low-Temperature Toughness of 1000 MPa Grade NiCrMoV Low Carbon Alloyed Steel |
| ZHOU Cheng, ZHAO Tan, YE Qibin, TIAN Yong, WANG Zhaodong, GAO Xiuhua |
| 图4 NiCrMoV低碳合金钢在不同温度回火后的XRD谱及残余奥氏体体积分数 |
| Fig.4 XRD spectra (a) and volume fraction of retained austenite (b) in the NiCrMoV low carbon alloyed steel tempered at different temperatures |
|