热轧硅钢表层动态再结晶区形成规律及剪切织构特征 |
| 姜伟宁, 武晓龙, 杨平, 顾新福, 解清阁 |
|
Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel |
| JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge |
| 图5 88%热轧压下量Fe-2.5Si-0.8Al样品全厚侧面区域3的EBSD分析 |