热轧硅钢表层动态再结晶区形成规律及剪切织构特征 |
| 姜伟宁, 武晓龙, 杨平, 顾新福, 解清阁 |
|
Formation of Dynamic Recrystallization Zone and Characteristics of Shear Texture in Surface Layer of Hot-Rolled Silicon Steel |
| JIANG Weining, WU Xiaolong, YANG Ping, GU Xinfu, XIE Qingge |
| 图2 88%压下量时Fe-2.5Si-0.8Al热轧板半厚侧面的EBSD分析 |
| Fig.2 EBSD analyses of semithick Fe-2.5Si-0.8Al hot-rolled sheets with 88% reduction (a) inverse pole figure (IPF) map (b) orientation distribution (c) orientation distribution function (ODF), φ2 = 45° (φ1, Φ, φ2—Euler angles in orientation space) |
|