开孔多孔金属材料在电催化及生物医用领域的研究进展 |
| 徐文策, 崔振铎, 朱胜利 |
|
Recent Advances in Open-Cell Porous Metal Materials for Electrocatalytic and Biomedical Applications |
| XU Wence, CUI Zhenduo, ZHU Shengli |
| 图1 脱合金法制备多孔金属材料示意图 |
| Fig.1 Schematic of the preparation of porous metal by dealloying method |
|