Al-AlN异构纳米复合材料的组织构型与热稳定性 |
| 聂金凤, 伍玉立, 谢可伟, 刘相法 |
|
Microstructure and Thermal Stability of Heterostructured Al-AlN Nanocomposite |
| NIE Jinfeng, WU Yuli, XIE Kewei, LIU Xiangfa |
| 图6 Al-AlN异构纳米复合材料热暴露前后的力学性能 |
| Fig.6 Mechanical properties of heterostructured Al-AlN nanocomposite before and after thermal exposure (a) variation of microhardness versus the thermal exposure time at 350oC (b) engineering stress-strain curves after exposure at 500oC for different holding time (c) ultimate tensile strength (UTS), yield strength (YS), and elongation (δ) variation curves of the composites with the exposure time |
|