Al-AlN异构纳米复合材料的组织构型与热稳定性 |
| 聂金凤, 伍玉立, 谢可伟, 刘相法 |
|
Microstructure and Thermal Stability of Heterostructured Al-AlN Nanocomposite |
| NIE Jinfeng, WU Yuli, XIE Kewei, LIU Xiangfa |
| 图3 AlN及AlN/Al基体界面结构的HRTEM表征 |
| Fig.3 HRTEM characterizations of AlN and the AlN/Al matrix interface structure (a, b) HRTEM images of AlN particles (c) HRTEM image of the green square in Fig.3b showing the metallurgical atomic bonding and matching between AlN and Al matrix (d-f) HRTEM images of the red square and yellow squares in Fig.3b showing the atomic plane spacing of the Al matrix and the AlN nanoparticles (d—interplanar spacing) |
|