层状异构Mg-3Gd合金的微观组织和力学性能 |
| 罗旋, 韩芳, 黄天林, 吴桂林, 黄晓旭 |
|
Microstructure and Mechanical Properties of Layered Heterostructured Mg-3Gd Alloy |
| LUO Xuan, HAN Fang, HUANG Tianlin, WU Guilin, HUANG Xiaoxu |
| 图5 不同微观结构AZ31镁合金的屈服强度与均匀延伸率的关系(基于文献[ |
| Fig.5 Uniform elongation versus yield strength of AZ31 alloy plotted based on the experimental data reported in Ref.[ |
|