层状异构Mg-3Gd合金的微观组织和力学性能 |
| 罗旋, 韩芳, 黄天林, 吴桂林, 黄晓旭 |
|
Microstructure and Mechanical Properties of Layered Heterostructured Mg-3Gd Alloy |
| LUO Xuan, HAN Fang, HUANG Tianlin, WU Guilin, HUANG Xiaoxu |
| 图4 不同微观结构和晶粒尺寸Mg-3Gd合金的屈服强度与均匀延伸率的关系 |
| Fig.4 Uniform elongation versus yield strength of Mg-3Gd alloy with different microstructures and average grain sizes |
|