热挤压与热处理对网状TiBw/TC18复合材料组织及性能的影响 |
| 陈润, 王帅, 安琦, 张芮, 刘文齐, 黄陆军, 耿林 |
|
Effect of Hot Extrusion and Heat Treatment on the Microstructure and Tensile Properties of Network Structured TiBw/TC18 Composites |
| CHEN Run, WANG Shuai, AN Qi, ZHANG Rui, LIU Wenqi, HUANG Lujun, GENG Lin |
| 图1 烧结态复合材料OM像、挤压棒材EBSD分析取样位置及挤压态材料热处理过程示意图 |
| Fig.1 OM image of as-sintered 2.0%TiBw/TC18 composites (a), schematic illustrating samples' locations of as-extruded 1.0%TiBw/TC18 for EBSD analysis (b), schematics of solution aging (c) and triple-annealing (d) treatments for as-extruded alloy and composites (AC—air cooling, FC—furnace cooling) |
|