突破强度-导电率制约关系:晶粒异构设计 |
| 侯嘉鹏, 孙朋飞, 王强, 张振军, 张哲峰 |
|
Breaking the Trade-Off Relation Between Strength and Electrical Conductivity: Heterogeneous Grain Design |
| HOU Jiapeng, SUN Pengfei, WANG Qiang, ZHANG Zhenjun, ZHANG Zhefeng |
| 图8 高强高导金属线材晶粒异构设计原理示意图 |
| Fig.8 Schematic of heterogeneous grain design principle for metallic metal wire achieving high strength and high electrical conductivity |
|