高熵合金跨尺度异构强韧化及其力学性能研究进展 |
| 安子冰, 毛圣成, 张泽, 韩晓东 |
|
Strengthening-Toughening Mechanism and Mechanical Properties of Span-Scale Heterostructure High-Entropy Alloy |
| AN Zibing, MAO Shengcheng, ZHANG Ze, HAN Xiaodong |
| 图13 粗晶、表面机械研磨处理(SMAT)和SMAT +时效处理样品拉伸力学性能[ |
| Fig.13 Tensile properties for coarse grain (CG), SMAT and SMAT-aged samples[ (a) engineering stress-strain curves (b) hardening rate and true stress as a function of true strain |
|