高熵合金跨尺度异构强韧化及其力学性能研究进展 |
| 安子冰, 毛圣成, 张泽, 韩晓东 |
|
Strengthening-Toughening Mechanism and Mechanical Properties of Span-Scale Heterostructure High-Entropy Alloy |
| AN Zibing, MAO Shengcheng, ZHANG Ze, HAN Xiaodong |
| 图8 Ni32.8Fe21.9Co21.9Cr10.9Al7.5Ti5.0高熵合金显微结构与拉伸力学性能[ |
| Fig.8 Microstructure and mechanical properties of Ni32.8Fe21.9Co21.9Cr10.9Al7.5Ti5.0 alloy[ (a) TEM image and the size distributions of L12 phase and fcc matrix (b) tensile properties of Ni32.8Fe21.9Co21.9Cr10.9Al7.5Ti5.0 alloy at room temperature (CNL—coherent nanolamellar) (c) TEM images of Ni32.8Fe21.9Co21.9Cr10.9Al7.5Ti5.0 alloy at different tensile strains |
|