高熵合金跨尺度异构强韧化及其力学性能研究进展 |
| 安子冰, 毛圣成, 张泽, 韩晓东 |
|
Strengthening-Toughening Mechanism and Mechanical Properties of Span-Scale Heterostructure High-Entropy Alloy |
| AN Zibing, MAO Shengcheng, ZHANG Ze, HAN Xiaodong |
| 图1 异构高熵合金与传统合金以及均质高熵合金材料的强度-塑性对比[ |
| Fig.1 Comparison of strength and ductility of high-entropy alloys (HEAs) with other conventional alloys and homogeneous HEAs[ |
|