从局域应力/应变视角理解异构金属材料的强韧化行为 |
| 范国华, 缪克松, 李丹阳, 夏夷平, 吴昊 |
|
Unraveling the Strength-Ductility Synergy of Heterostructured Metallic Materials from the Perspective of Local Stress/Strain |
| FAN Guohua, MIAO Kesong, LI Danyang, XIA Yiping, WU Hao |
| 图3 异构金属材料的强化机制[ |
| Fig.3 The strengthening mechanism of heterostructured metallic materials[ (a) pile-ups of geometrically necessary dislocations (GNDs) (b) strain and strain gradient versus distance from the domain interface (c) local stress versus distance from the domain interface |
|