| 范国华, 缪克松, 李丹阳, 夏夷平, 吴昊 |
|
Unraveling the Strength-Ductility Synergy of Heterostructured Metallic Materials from the Perspective of Local Stress/Strain |
| FAN Guohua, MIAO Kesong, LI Danyang, XIA Yiping, WU Hao |
| 图2 异构金属材料的多个变形阶段[ |
| Fig.2 The multi-stages of deformation in heterostructured metallic materials (a) three deformation stages of heterostructured metallic materials[ (b) lattice strain evolution of Ti/Al layered heterostructured materials measured by neutron diffraction[ |
|