从局域应力/应变视角理解异构金属材料的强韧化行为 |
| 范国华, 缪克松, 李丹阳, 夏夷平, 吴昊 |
|
Unraveling the Strength-Ductility Synergy of Heterostructured Metallic Materials from the Perspective of Local Stress/Strain |
| FAN Guohua, MIAO Kesong, LI Danyang, XIA Yiping, WU Hao |
| 图1 几种典型的异构设计策略及其强韧化效果[ |
| Fig.1 Typical heterostructured architectures and their effects on strength and ductility synergy (a, b) gradient heterostructure (FG and CG are referred to fine grain and coarse grain, respectively)[ |
|