金属材料的构型化复合与强韧化 |
| 范根莲, 郭峙岐, 谭占秋, 李志强 |
|
Architecture Design Strategies and Strengthening-Toughening Mechanisms of Metal Matrix Composites |
| FAN Genlian, GUO Zhiqi, TAN Zhanqiu, LI Zhiqiang |
| 图4 CNT/2024Al基体三峰异构复合材料[ |
| Fig.4 CNT/2024Al trimodal composites[ (a-d) typical three-level grain structures and the grain size distribution (e, f) tensile strength and ductility of CNT/2024Al with different grain structures |
|