异构金属材料的设计与制造 |
| 张显程, 张勇, 李晓, 王梓萌, 贺琛贇, 陆体文, 王晓坤, 贾云飞, 涂善东 |
|
Design and Manufacture of Heterostructured Metallic Materials |
| ZHANG Xiancheng, ZHANG Yong, LI Xiao, WANG Zimeng, HE Chenyun, LU Tiwen, WANG Xiaokun, JIA Yunfei, TU Shantung |
| 图11 自下而上设计法及其主要工艺参数[ |
| Fig.11 Schematics of the bottom-up design method and their main process parameters (a) electrodeposition (ED)[ |
|