异构金属材料的设计与制造 |
| 张显程, 张勇, 李晓, 王梓萌, 贺琛贇, 陆体文, 王晓坤, 贾云飞, 涂善东 |
|
Design and Manufacture of Heterostructured Metallic Materials |
| ZHANG Xiancheng, ZHANG Yong, LI Xiao, WANG Zimeng, HE Chenyun, LU Tiwen, WANG Xiaokun, JIA Yunfei, TU Shantung |
| 图8 异质金属材料制造技术手段的分类原理图 |
| Fig.8 Classification schematic of precise preparation techniques of heterogeneous metal materials |
|