异构金属材料的设计与制造
张显程, 张勇, 李晓, 王梓萌, 贺琛贇, 陆体文, 王晓坤, 贾云飞, 涂善东

Design and Manufacture of Heterostructured Metallic Materials
ZHANG Xiancheng, ZHANG Yong, LI Xiao, WANG Zimeng, HE Chenyun, LU Tiwen, WANG Xiaokun, JIA Yunfei, TU Shantung
图7 孪晶厚度对多级孪晶金属力学性能的影响[76,77]
Fig.7 Effects of twin thickness on mechanical properties for hierarchical nanotwinned metals
(a) effect of secondary twin thickness (L2) with D on transition twin thickness (L1Tr)[76]
(b) effect of L2 on average flow stress[77] (L1—primary twin thickness)