异构金属材料的设计与制造 |
| 张显程, 张勇, 李晓, 王梓萌, 贺琛贇, 陆体文, 王晓坤, 贾云飞, 涂善东 |
|
Design and Manufacture of Heterostructured Metallic Materials |
| ZHANG Xiancheng, ZHANG Yong, LI Xiao, WANG Zimeng, HE Chenyun, LU Tiwen, WANG Xiaokun, JIA Yunfei, TU Shantung |
| 图6 微观结构参数对纳米孪晶金属力学性能的影响[ |
| Fig.6 Effects of microstructure parameters on mechanical properties for nanotwinned metals (a) effect of twin thickness on stress-strain curves[ (b) effect of twin thickness (λ) or grain size (D) for nanocrystalline Cu on strain rate sensitivity index (m)[ (c) effect of stacking fault energy on stress-strain curves[ (d) effect of the angle between loading axis and twin boundary (θ) on the ratio of critical stress for dislocation emission and shear modulus[ |
|