纳米金属结构材料的韧化
赵永好, 毛庆忠

Toughening of Nanostructured Metals
ZHAO Yonghao, MAO Qingzhong
图10 超细晶高锰钢的拉伸曲线和X-射线衍射谱[89]
Fig.10 Tensile curves (a) and X-ray diffraction spectra (b) of ultrafine grained Fe-Mn alloy[89]