纳米金属结构材料的韧化 |
| 赵永好, 毛庆忠 |
|
Toughening of Nanostructured Metals |
| ZHAO Yonghao, MAO Qingzhong |
| 图9 高纯、致密bi-modal和multi-modal镍的微观结构和拉伸曲线以及屈服强度-断裂延伸率对比[ |
| Fig.9 Microstructures (a, b) and tensile curves (c) of high-purity and dense bi/multi-modal nickel (Bi-Ni/multi-Ni) and review of yield strength-tensile ductility of nickel (d)[ |
|