纳米金属结构材料的韧化 |
| 赵永好, 毛庆忠 |
|
Toughening of Nanostructured Metals |
| ZHAO Yonghao, MAO Qingzhong |
| 图4 陶瓷、金属和有机高分子材料拉伸曲线示意图以及静态韧性与强度、断裂延伸率、加工硬化率的关系 |
| Fig.4 Schematic of tensile curves of ceramics, metals, and organic polymers and the relationship between static toughness and strength, fracture elongation, and work hardening rate (PMCs—polymer matrix composites; ε—strain, σ—stress) |
|