SUS316不锈钢马鞍形管-管接头的残余应力数值模拟及高效计算方法开发 |
| 骆文泽, 胡龙, 邓德安 |
|
Numerical Simulation and Development of Efficient Calculation Method for Residual Stress of SUS316 Saddle Tube-Pipe Joint |
| LUO Wenze, HU Long, DENG Dean |
| 图13 周向残余应力沿中心线分布(90°截面上不同焊层完成后) |
| Fig.13 Hoop residual stress distributions along the welding centerline in 90° section after welding at different layers (Inset shows the measuring direction) |
|