Al-Li合金中 δ′/θ′/δ′复合沉淀相结构演化及稳定性的第一性原理探究
王硕, 王俊升

Structural Evolution and Stability of the δ′/θ′/δ′ Composite Precipitate in Al-Li Alloys: A First-Principles Study
WANG Shuo, WANG Junsheng
表3 位于3种θ′/δ′界面处,不同原子对化学键的键长 (nm)
Table 3 Summaries of the bond lengths of different atomic interactions in three types of θ′/δ′ interfaces
StructureLi1—Al2Li1—Al3Al1—Al2Al1—Al3
In-phase #20.2880.2880.2880.288
Anti-phase a / 2[010]0.3860.2710.2620.397
Anti-phase a / 2[110]0.2800.2800.2790.279