Al-Li合金中 δ′/θ′/δ′复合沉淀相结构演化及稳定性的第一性原理探究
王硕, 王俊升

Structural Evolution and Stability of the δ′/θ′/δ′ Composite Precipitate in Al-Li Alloys: A First-Principles Study
WANG Shuo, WANG Junsheng
表2 基于Rose断裂模型拟合得到的3种界面结构的临界位移(dic),解理功(Gc)以及理想解理应力(σic)
Table 2 Critical spacing (dic), cleavage energy (Gc), and the ideal cleavage stress (σic) for three interfacial structures with different phase relationships evaluated by RGS model under tensile deformation
Structuredic / nmGc / (J·m-2)σic / GPa
In-phase #20.0591.94812.356
Anti-phase a / 2[010]0.0501.3419.796
Anti-phase a / 2[110]0.0612.09712.659