Al-Li合金中 δ′/θ′/δ′复合沉淀相结构演化及稳定性的第一性原理探究
王硕, 王俊升

Structural Evolution and Stability of the δ′/θ′/δ′ Composite Precipitate in Al-Li Alloys: A First-Principles Study
WANG Shuo, WANG Junsheng
表1 3种界面结构的界面面积、界面能以及解理面各相的表面能
Table 1 Calculated interface area (S), interfacial energy (γinterface), and relative surface energy (γsurface) of three cleavage planes with different phase relationships
StructureS / nm2γsurfaceθ' / (J·m-2)γsurfaceδ' / (J·m-2)γinterface / (J·m-2)
In-phase #20.1651.4010.8940.335
Anti-phase a / 2[010]0.1631.4180.8940.964
Anti-phase a / 2[110]0.1631.4450.846-0.015