Al-Li合金中 δ′/θ′/δ′复合沉淀相结构演化及稳定性的第一性原理探究
王硕, 王俊升

Structural Evolution and Stability of the δ′/θ′/δ′ Composite Precipitate in Al-Li Alloys: A First-Principles Study
WANG Shuo, WANG Junsheng
图7 3种θ'/δ'界面结构的键能-位移曲线以及对应的解理应力变化曲线
Fig.7 Bonding energy (Eb)-displacement (d) curves for three θ'/δ' interface structures (a) and corres-ponding cleavage stress variation curves (b)