非晶态U60Fe27.5Al12.5 合金的晶化动力学行为 |
| 韩录会, 柯海波, 张培, 桑革, 黄火根 |
|
Kinetic Crystallization Behavior of Amorphous U60Fe27.5Al12.5 Alloy |
| HAN Luhui, KE Haibo, ZHANG Pei, SANG Ge, HUANG Huogen |
| 图5 U60Fe27.5Al12.5非晶合金在不同温度退火后的DSC晶化曲线及晶化体积分数随温度的变化曲线 |
| Fig.5 DSC curves (a) and plots of x (b) as a function of the annealing temperature (t) of U60Fe27.5Al12.5 amorphous alloy annealed at different temperatures |
|